Inti EPC Ferit

Inti EPC Ferit

product-351-290

 

POLA

G.W

UKURAN (mm)

A

BM

C

D

E

F

G

Hmm

EPC13

2.5

13.3±0.3

8.3

5.6±0.2

4.6±0.2

4.5±0.2

6.6±0.2

2.1±0.1

10.5

EPC17.8

5.6

17.8±0.4

11.5

7.4±0.2

6.0±0.2

6.0±0.2

8.7±0.2

2.8±0.1

14.3

EPC34

62

34.0±0.5

19.7

14.5±0.2

14.5±0.2

16.4±0.2

20.9±0.2

9.1±0.2

24.8

EPC39

78

39.0±0.7

24.7

17.6±0.3

15.5±0.2

14.1±0.3

19.6±0.2

9.7±0.1

30.5

EPC41

108

41.0±0.6

23.6

18.5±0.2

16.5±0.2

18.9±0.2

24.5±0.2

11.0±0.2

28.8

 

POLA

PARAMETER

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lem

Aem2

baiklah3

ZP40

EPC13

2.46

30.6

12.5

382.0

870

2.1

EPC17.8

1.77

40.2

22.7

917.0

1200

4.5

EPC34

0.73

89.6

122.6

10985.0

3200

56.0

EPC39

0.60

87.95

147.0

12960.0

3700

70.5

EPC41

0.57

104.1

183.2

19064.0

4100

97.0